Categories: CARBON STEEL PIPE/TUBE
|
Grade |
C(Max) | Mn | Si(Min) | P(Max) |
S(Max) |
|
A1 |
0.27 | Max.0.93 | 0.10 | 0.035 | 0.035 |
| C | 0.35 | 0.29~1.06 | 0.10 | 0.035 |
0.035 |
| Grade | Tensile Strength(Mpa) | Yield Strength(Mpa) | Elongation (%) |
| A1 | ≥ 415 | ≥ 255 | ≥ 30 |
| C | ≥ 485 | ≥ 275 | ≥ 30 |
|
Hot rolled |
Outside Diameter, mm |
Tolerance, mm |
|
OD≤101.6 |
+0.4/-0.8 |
|
|
101.6<OD≤127 |
+0.4/-1.2 |
|
|
Cold Drawn |
Outside Diameter, mm |
Tolerance, mm |
|
OD<25.4 |
±0.10 | |
|
25.4≤OD≤38.1 |
±0.15 |
|
|
38.1<OD<50.8 |
±0.20 |
|
|
50.8≤OD<63.5 |
±0.25 |
|
|
63.5≤OD<76.2 |
±0.30 |
|
|
76.2≤OD≤101.6 |
±0.38 |
|
|
101.6<OD≤127 |
+0.38/-0.64 |
|
Hot rolled |
Outside Diameter , mm |
Tolerance, % |
|
OD≤101.6, WT≤2.4 |
+40/-0 | |
|
OD≤101.6, 2.4<WT≤3.8 |
+35/-0 |
|
|
OD≤101.6, 3.8<WT≤4.6 |
+33/-0 |
|
|
OD≤101.6, WT>4.6 |
+28/-0 |
|
|
OD>101.6, 2.4<WT≤3.8 |
+35/-0 |
|
|
OD>101.6, 3.8<WT≤4.6 |
+33/-0 |
|
| OD>101.6, WT>4.6 |
+28/-0 |
|
|
Cold Drawn |
Outside Diameter , mm |
Tolerance, % |
|
OD≤38.1 |
+20/-0 |
|
|
OD>38.1 |
+22/-0 |