Chemical Compositions(%) of 12Cr1MoV:
Elements | Data |
Carbon | 0.08-0.15 |
Silicon | 0.17-0.37 |
Manganese | 0.40-0.70 |
Phosphorus(max) | ≤0.030 |
Sulfur(max) | ≤0.030 |
Chromium | 0.90-1.20 |
Molybdenum | 0.25-0.35 |
Cuprum(max) | ≤0.20 |
Nickel(max) | ≤0.30 |
Vanadium(max) | 0.15-0.30 |
Mechanical Properties of 12Cr1MoV:
Yield Strength (Mpa) | 470-640 |
Tensile Strength (Mpa) | 255 |
Elongation (%) | 21 |
The W.T. tolerance of 12Cr1MoV:
W.T.(S) | Tolerance of W.T. | |
<3.5 | +15%(+0.48mm min) | |
-10%(+0.32mm min) | ||
3.5-20 | +15%,-10% | |
>20 | D<219 | ±10% |
D≥219 | +12.5%,-10% |